Abstract:

Austenitic stainless steel offer great imperviousness to general erosion because of the development of a detached surface film. They are broadly utilized as a part of the sustenance and concoction preparing ventures and in addition in biomaterial applications. In any case, they can experience the ill effects of setting erosion in chloride particle containing arrangements. All things considered, in the meantime they have discovered little use in mechanical building applications in view of their low hardness and poor wear resistance. In this examination work, to enhance the previously mentioned reasons, surface solidifying by Flame hardening procedure is done. It has for some time been an outstanding a warm treatment for enhancing the surface properties of austenitic stainless steel. The examples were fire solidified for 5 minutes, 10 minutes and 15 minutes separately. Wear test for every one of the examples were completed by stick on plate testing process. The outcomes were contrasted and an untreated specimen and finished up with metallographic tests like optical tiny tests and examining electron magnifying lens tests.

Cite This Article:
Show All (MLA | APA | Chicago | Harvard | IEEE | Bibtex)
Share: